BULK ORDERS · OEM/ODM AVAILABLE• 316L SURGICAL STEEL • 15+ YEARS EXPERTISE• CNC PRECISION ±0.05mm• EU REACH CERTIFIED•

Nickel Release Standards

The single most important compliance question for body piercing and skin-contact jewelry in the European market.

Nickel is the most common cause of contact allergy in the industrialised world. For jewelry sold into markets that regulate it, nickel release is not a quality preference - it is a legal requirement that arrives with the product.

What nickel release actually means

The concern is not whether a material contains nickel. Most stainless steel does. The concern is whether nickel can migrate out of the material and onto skin in a quantity large enough to sensitise the wearer.

This distinction is why a part can contain nickel and still pass: in a correctly produced austenitic stainless steel, nickel is locked into the alloy's crystal structure rather than sitting available at the surface.

The EU regulatory framework

Nickel is restricted under REACH Annex XVII, entry 27. Two thresholds matter for jewelry:

Applies toLimitUnit
Piercing post assemblies0.2µg/cm²/week
Articles in prolonged skin contact0.5µg/cm²/week
These are the standard industry limitsThe figures above - 0.2 µg/cm²/week for piercing post assemblies and 0.5 µg/cm²/week for articles in prolonged skin contact - are the limits the jewelry industry tests against as a matter of routine. We test to them and report the measured release figure for the batch, rather than relying on a material declaration. Where a market applies a transitional provision to a particular article type, that is confirmed at the enquiry stage.

How compliance is tested

Worn-condition claimsIf you are claiming compliance for an item that will be worn, ask for EN 12472 followed by EN 1811. An EN 1811 result on a new, unworn sample describes a different object from the one your customer will be wearing in six months.

Why 316L is the default grade

In 316L, nickel is bound within the austenitic grain structure and stabilised by molybdenum. Release from a correctly finished 316L surface is therefore low enough that the grade has been the standard choice for implants and piercing hardware for decades. That is a property of the alloy and the finish together - neither one alone is sufficient.

What makes a part fail

What to require from a supplier

  1. Grade on the paperwork

    The alloy grade must appear on the purchase order, on the mill certificate, and on the packing documents - consistently.

  2. A test report naming your part

    Ask for an EN 1811 report from an accredited laboratory that identifies the specific article tested, not a generic material declaration.

  3. Worn-condition testing where relevant

    EN 12472 plus EN 1811 for anything that will be worn against skin for extended periods.

  4. Batch traceability

    The report should link to the production batch you actually receive, with a date you can check.

A report is not a certificateA test report covers the samples tested on the date stated. It is not a blanket guarantee covering every unit you will ever receive. Ask how often re-testing is performed and how production batches are tied back to reports before you build a market claim on it.

Need this specified for your order?

Send us your drawing, sample or technical requirement. We will confirm feasibility, tolerances and price in writing before production.

Request a Quote