Buyers are often quoted 304 as a cheaper alternative and told the difference does not matter. It does matter, and the reason is a single alloying element.
Chemical composition
| Element | 304 | 316L |
|---|---|---|
| Chromium | 18–20% | 16–18% |
| Nickel | 8–10.5% | 10–14% |
| Molybdenum | — | 2–3% |
| Carbon (max) | 0.08% | 0.03% |
| Manganese (max) | 2% | 2% |
| Iron | Balance | Balance |
Why molybdenum is the deciding factor
Molybdenum is the element that separates the two grades. It substantially improves resistance to pitting and crevice corrosion in chloride environments - which, for jewelry, means sweat, seawater and chlorinated water. Grade 304 contains no molybdenum at all. That single difference is the entire reason 316L became the default for skin-contact, body-piercing and implant applications.
Skin contact and nickel
Both grades contain nickel, and neither is nickel-free. What differs is how readily that nickel can migrate out of the surface and onto skin. In practice, release depends on the alloy, the surface finish and the environment. 316L is the grade used for surgical implants and is the safer default wherever nickel sensitivity is a commercial or regulatory concern.
Compliance is demonstrated by testing, not by grade alone. A supplier claiming 316L is not the same as a supplier holding a nickel release test report for the part you are buying. See our guide to nickel release standards for the test methods involved.
When 304 is still a reasonable choice
- Display stands, packaging hardware and other non-skin-contact components
- Budget promotional pieces where the buyer knowingly accepts a shorter service life
- Applications with no chloride exposure and no market that requires nickel release testing
Reasonable does not mean equivalent. If the item goes against skin in a regulated market, the grade choice is not really a cost decision - it is a compliance decision.
Cost and sourcing
316L carries a higher material cost, driven by the molybdenum content and the tighter carbon control. The gap moves with nickel and molybdenum market prices, so a figure quoted last quarter is not reliable this quarter.
For a finished piece, the material premium is usually a smaller share of total cost than buyers expect. Machining, polishing, coating and inspection dominate the unit price on a small precision part. Ask for a side-by-side quote on your specific design rather than assuming 304 is proportionally cheaper.
How to specify the grade
- State the grade explicitly on the purchase order - 316L per ASTM A276, or EN 1.4404 in European terms
- Require mill certificates (material test reports) with the shipment, not on request only
- Require XRF verification on finished goods where the application is regulated
- For piercing items, add the nickel release requirement and the test standard to the PO
- Name the surface finish separately - grade and finish are two different specifications
Need this specified for your order?
Send us your drawing, sample or technical requirement. We will confirm feasibility, tolerances and price in writing before production.
Request a Quote