Layer thickness is one of the most quoted and least examined specifications in jewelry manufacturing. This guide covers the units, the measurement methods, and the one question that exposes most confused reports.

The units, and how they convert

UnitSymbolConversion
Micrometreµm1 µm = 0.001 mm
Microinchµin1 µm ≈ 39.37 µin
Milmil1 mil = 25.4 µm (not the same as a millimetre)
The classic mix-upA report quoting 0.5 mil and one quoting 0.5 µm differ by a factor of roughly fifty. Always confirm the unit in writing, especially when comparing quotes from suppliers in different regions.

The total film trap

This is where most confusion starts. On a PVD coating, the total film may consist of a bond layer, a colour layer and a top layer. On decorative PVD for stainless steel jewelry, that total typically runs 0.03 - 0.1 µm - comfortably under one micron - so a report quoting a total film of one micron is describing a different class of coating altogether. Even within the correct range, a total figure tells you nothing about how much material actually sits in the colour layer, which is the layer that determines the appearance and the wear behaviour.

The same applies to multi-layer electroplating, where a nickel barrier layer and a top layer are deposited separately. A single headline number can be technically true and commercially meaningless.

The questions that resolve it

How XRF measurement works

X-ray fluorescence is a non-destructive method. X-rays excite the atoms in the coating, and the emitted spectrum identifies which elements are present and estimates how thick the layer is. It is fast, it works on finished parts, and it can be repeated on the same piece.

Its limitations

Cross-section microscopy is destructive but more definitive: the part is mounted, cut, polished and examined under magnification, and each layer is measured directly. Where the stakes are high, this is the method that settles a disagreement.

Reading a report properly

  1. Check the unit

    Micrometres, microinches or mils. Confirm which, in writing.

  2. Check which layer

    Total film and colour layer are different specifications.

  3. Check the method

    XRF and cross-section are not interchangeable, and they do not always agree.

  4. Check the sample

    Worn-condition testing and new-part testing answer different questions.

  5. Check the tolerance

    A number without an acceptance range is not a specification you can inspect against.

A single number is not a specificationA layer thickness without a measurement method, a sample location and a tolerance is not something you can accept or reject a shipment against. Any supplier who cannot state all three is not giving you a specification.

Need this specified for your order?

Send us your drawing, sample or technical requirement. We will confirm feasibility, tolerances and price in writing before production.

Request a Quote
中文