PVD is the finish behind almost every gold-toned stainless steel jewelry piece on the market. It is widely described but rarely explained. Here is the process, the testing, and the honest limits.
1. How PVD coating works
Physical Vapour Deposition is a vacuum coating process. Where electroplating deposits metal out of a liquid chemical bath, PVD builds the coating atom by atom from a solid source inside a sealed chamber. Nothing about the part touches liquid chemistry.
The process, step by step
- Substrate preparation
Parts are machined, then polished, degreased and ultrasonically cleaned. This stage decides the final appearance: PVD is a conformal coating, so it follows the surface underneath rather than filling it in. A mirror-polished part stays mirror-polished; a brushed part keeps its grain.
- Chamber loading and evacuation
Parts are mounted on rotating fixtures inside the vacuum chamber. Air is pumped out to create the high-vacuum environment the process needs.
- Target vaporisation
A solid metal target is vaporised - by arc evaporation or by sputtering. The target material determines the final colour family: titanium, zirconium, chromium or aluminium.
- Reaction and deposition
A reactive gas is introduced - nitrogen, acetylene or oxygen. The vaporised metal reacts with it and lands on the parts as a hard ceramic compound. Gold tones come from titanium nitride or zirconium nitride; black from carbon-based coatings; rose and gunmetal tones from adjusted gas ratios and alloy targets.
- Cooling and inspection
Parts cool under vacuum, then are checked for colour consistency, coverage in recessed areas, and surface defects.
What the process means for the finished part
| Property | PVD | Electroplating |
|---|---|---|
| Deposition | Vacuum, dry process | Liquid chemical bath |
| Waste water | None | Significant |
| Typical coating thickness | 0.03 - 0.1 µm (total film) | Several microns |
| Hardness | Generally higher than the 316L substrate | Lower |
| Colour range | Gold, rose, black, gunmetal, blue, rainbow | Limited by available metal salts |
| Adhesion | High, when substrate prep is correct | Moderate |
2. Salt spray and durability testing
Coating performance is verified with standardised tests rather than with adjectives. The table below lists what we test, the standard each test follows, and what the result actually tells you.
| Test | Standard | What it measures |
|---|---|---|
| Neutral Salt Spray (NSS) | ISO 9227 / ASTM B117 | Corrosion resistance and coating integrity under continuous salt exposure |
| Coating adhesion (cross-cut) | ISO 2409 | How well the coating bonds to the 316L substrate |
| Nickel release | EN 1811 (with EN 12472 for worn articles) | Nickel migration to skin - the compliance test for skin-contact and piercing items |
| Layer thickness | XRF (X-ray fluorescence) | Elemental layer thickness, measured non-destructively |
How the salt spray test is run
- Test conditions: 5% sodium chloride solution at 35 °C, continuous spray, per ISO 9227
- Standard run duration: 96 hours of continuous neutral salt spray
- Samples are drawn from the production batch itself, not from a separately prepared golden sample
- Parts are assessed at agreed intervals for blistering, discolouration, peeling and substrate corrosion
- Results are recorded per batch and retained for traceability
What affects the result
- Substrate finish - a mirror-polished surface holds a more uniform coating than a brushed or sandblasted one
- Geometry - recessed areas, sharp internal corners and deep engraving are harder to coat evenly
- Colour - dark and black coatings behave differently from gold tones under the same conditions
- Post-coating handling - skin oils, abrasive packaging and metal-on-metal contact accelerate wear
3. Care and maintenance
A PVD finish is durable but not indestructible. A few consistent habits will keep the appearance intact far longer than any single product can.
Daily care
- Wipe with a soft, dry or slightly damp cloth after wearing - body oils and sunscreen residue are the most common cause of dulling
- For a deeper clean, use lukewarm water with a drop of mild pH-neutral soap, then pat dry with a soft cloth
- Dry the piece fully before storing it - trapped moisture in a closed box is what causes spotting
What to avoid
- Chlorinated pools, hot tubs and seawater - chlorine attacks the 316L substrate wherever the coating is breached
- Perfume, hairspray and sunscreen applied directly onto the piece - apply those first, let them dry, then put the jewelry on
- Abrasive cleaners, polishing compounds, silver dip and most ultrasonic cleaners
- Storing pieces loose together - metal-on-metal contact abrades the coating
Storage
Keep each piece in its own soft pouch or in a compartmented tray, in a dry place. Chains should be hung or laid flat rather than coiled tightly, which puts stress on the links and the clasp.
If the finish dulls
Light surface dulling usually comes off with a soft cloth. Once the coating is visibly worn through to the substrate, restoring it is a production process rather than a polishing job - contact us with photos and we will assess whether re-polishing and re-coating is practical.
Need this specified for your order?
Send us your drawing, sample or technical requirement. We will confirm feasibility, tolerances and price in writing before production.